Quentin Nguyen
Industrial
- Apr 20, 2023
- 14
Dear engineers,
It is the first time I design a thick wall expansion joint follow ASME sec VIII div 1 to get U Stamp for the heat exchanger.
I am confusing the material use for calculate and fabricate the expansion joint.
Is it SA-240 304 or SA-182 F 304?
I'm using SA-182, but the search result on the internet show SA-240 (plate type).
Dose someone here has experience on this part?
Thank you so much for the help.
It is the first time I design a thick wall expansion joint follow ASME sec VIII div 1 to get U Stamp for the heat exchanger.
I am confusing the material use for calculate and fabricate the expansion joint.
Is it SA-240 304 or SA-182 F 304?
I'm using SA-182, but the search result on the internet show SA-240 (plate type).
Dose someone here has experience on this part?
Thank you so much for the help.