Hello,
I am fabricating Kettle type heat exchanger from contractor whose specification are as follows:
Service of Shell Side: LPG
Service of Tube Side: Steam
Minimum temperature of LPG : 50 Centigrade
Maximum temperature of LPG : 80 Centigrade
Minimum Allowable Working temperature of shell side: 15 Centigrade
Maximum Allowable Working temperature of shell side: 80 Centigrade
Shell material as per Drawing: R2 (As per Romanian Standard)
I want to know that what is equivalent ASTM standard of Romanian material R2. Also can i use ASTM 516 Gr70 as a shell material in place of ASTM A537 Class 2 in above mentioned conditions.
Als0, what are the minimum allowable temperature limit of ASTM 516 Gr 70 and ASTM A537 Class 2?
Thanks.
I am fabricating Kettle type heat exchanger from contractor whose specification are as follows:
Service of Shell Side: LPG
Service of Tube Side: Steam
Minimum temperature of LPG : 50 Centigrade
Maximum temperature of LPG : 80 Centigrade
Minimum Allowable Working temperature of shell side: 15 Centigrade
Maximum Allowable Working temperature of shell side: 80 Centigrade
Shell material as per Drawing: R2 (As per Romanian Standard)
I want to know that what is equivalent ASTM standard of Romanian material R2. Also can i use ASTM 516 Gr70 as a shell material in place of ASTM A537 Class 2 in above mentioned conditions.
Als0, what are the minimum allowable temperature limit of ASTM 516 Gr 70 and ASTM A537 Class 2?