I am currently reviewing our shop traveler for processing B7 studs. The final configuration of the part is an M12 thread X 4.5 in long with dacromet 320 coating.
The parts will be thread rolled in our facility. I am confused as to the proper sequencing of operations to achieve the correct mechanical properties.
Will there be any difference between the two process sequences below in the final configuration?
Seq. 1
Heat treat & quench per ASTM A193 B7
Blast scale
Thread Roll
Temper
Dacromet
Seq. 2
Thread roll
Heat treat & quench per ASTM A193 B7
Blast
Dacromet
I must confess that I am weak in metallurgy. I am unsure if the heat treat process would relieve internal stresses or if the tempering process is necessary in both sequences. There are testing processes in thos sequences.
Thanks in advance for all feedback
The parts will be thread rolled in our facility. I am confused as to the proper sequencing of operations to achieve the correct mechanical properties.
Will there be any difference between the two process sequences below in the final configuration?
Seq. 1
Heat treat & quench per ASTM A193 B7
Blast scale
Thread Roll
Temper
Dacromet
Seq. 2
Thread roll
Heat treat & quench per ASTM A193 B7
Blast
Dacromet
I must confess that I am weak in metallurgy. I am unsure if the heat treat process would relieve internal stresses or if the tempering process is necessary in both sequences. There are testing processes in thos sequences.