Feb 5, 2012 #1 QPAini Mechanical Jan 30, 2012 7 0 0 QA Any body know ASTM A27 (Fire Brick) material composition?
Feb 5, 2012 #2 metengr Materials Oct 2, 2003 15,478 0 0 US According to my source, ASTM A 27 is Standard Specification for Steel Castings, Carbon for General Application. Upvote 0 Downvote
According to my source, ASTM A 27 is Standard Specification for Steel Castings, Carbon for General Application.
Feb 5, 2012 #3 arunmrao Materials Oct 1, 2000 4,758 0 0 IN I agree with metengr, pl clarify if you need for standards reference firebrick . _____________________________________ "It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year Upvote 0 Downvote
I agree with metengr, pl clarify if you need for standards reference firebrick . _____________________________________ "It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
Feb 6, 2012 Thread starter #4 QPAini Mechanical Jan 30, 2012 7 0 0 QA I am sorry my friends, it's ASTM C27, not A27, please help Upvote 0 Downvote