qualitychow22
Civil/Environmental
- Aug 25, 2017
- 5
Hi Forum,
My supplier is handing me Mill Certs that conforms to ASTM 529 (carbon-manganese steel)for anchor bolts which should be fabricated and tested under ASTM F1554. I have both the ASTMs and it appears to me that F1554 has stringent quality manufacturing requirements than 529. There is not reference or relationships I can find with these ASTMs. ASTM 529 does not tie into fabricating anchor bolts... Has anyone have any thoughts on this?
Thanks!
My supplier is handing me Mill Certs that conforms to ASTM 529 (carbon-manganese steel)for anchor bolts which should be fabricated and tested under ASTM F1554. I have both the ASTMs and it appears to me that F1554 has stringent quality manufacturing requirements than 529. There is not reference or relationships I can find with these ASTMs. ASTM 529 does not tie into fabricating anchor bolts... Has anyone have any thoughts on this?
Thanks!