Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Available Thicknesses for Plates

Status
Not open for further replies.

GustavoR

Materials
Apr 19, 2007
9
Hello everyone;
I would appreciate if someone could tell if there exists a standard for available commercial thicknesses for PV&B plates equivalent to ASME B36.10M for pipe. And for tank plates?
Thank you.
 
Replies continue below

Recommended for you

It varies depending on the source. If buying sufficient quantities from a mill, you can get it rolled to any desired thickness. If buying stock plate from a distribution center, you will be limited to the thicknesses they stock.
 
Our supplier has by the 1/8" up to 2" thick, then by the 1/4" thereafter - I'm referring to SA-516 Gr70 plate.
 
From memory, SA-516-70 plate is generally available in 1/16" increments from 3/16" thick to 1/2" thick, 1/8" increments from 1/2" thick to 1 1/2" thick, and 1/4" increments above 1 1/2" thick.

-Christine
 
vesselfab,
Don't laugh we had 6 filter bodies fabricated where we used 12" Class 2500 flanges on the discharge end. The mating flange to the body flange was a cover plate with a 4" Class 2500 WNF attached and reinforced with a 3/16" thick plate of the appropriate material, duly attached with the required weep hole. The actual calculations submitted call for a 1/16" pad.
 