Flaiano
Industrial
- Dec 4, 2014
- 6
Good morning all,
regarding Figure 6.25 Fillet Weld Break and Macroetch Test Plate of the AWS D1.1 2020, does the value 5/16 in(leg fillet weld) mean a minimum?
Thank you very much for your reply
Have a nice weekend
Flaiano
regarding Figure 6.25 Fillet Weld Break and Macroetch Test Plate of the AWS D1.1 2020, does the value 5/16 in(leg fillet weld) mean a minimum?
Thank you very much for your reply
Have a nice weekend
Flaiano