My question to the experts is this- When preparing a prequalified wps for FCAW-G using E71T-9/0.045" wire and 75/25 shielding gas is it allowable for example to list amperage as 150 - 180 +/- 10% and voltage as 22.0 - 28.0 +/- 15% and travel speed as 4.0 - 10.0 ipm +/- 25%, provided these values fall within the manufactures recommendations for this wire/gas combination. Base material is a Group II. Thank you for your help.
 
Replies continue below

Recommended for you

The ranges listed by the WPS should already have the permitted ranges listed. Don't expect the welder to be a mathematician.

If you are new to writing WPSs, there is a three day seminar available. The next seminar is scheduled for October 2019. The contact for more information is listed in an AWS publication:"Inspection Trends". You can probably locate the AWS Website for the publication with a quick search of the internet.

I just did a search using the name of the seminar, "The Atlas of Welding Procedure Specifications" and found a couple of hits. The email address of the contact person is listed.

Best regards - Al
 
For "prequalified' the power supply must be constant voltage.

If you wanted consistent sound welds, probably not.
 