anolan23
Mechanical
- Apr 29, 2015
- 54
This unit shall be built to ASME B31.1. See the picture that shows the spool piece . The small flange is a socketweld and the larger one is a blind flange. There is an intermediate small pipe. I want to know if the distance between welds is an issue. If the closeness of the welds is an issue, does filling the space between help at all? Thank you