5pointslow
Mechanical
I am preparing a new WPS and PQR for P1 materials using GMAW with impact testing. These are prepared in accordance with ASME Sec.IX.
My question concerns the base metal thickness range qualified. I would like to use the same procedure and PQR to qualify material that is 0.154" thick up to 1" thick or more.
From what i have read, this will not be possible.
If I am correct in this conclusion, can I use two PQRs to increase the range qualified on the WPS?
How do I determine if I use the minimum thickness values of QW-403.6 or QW-451.1?
My question concerns the base metal thickness range qualified. I would like to use the same procedure and PQR to qualify material that is 0.154" thick up to 1" thick or more.
From what i have read, this will not be possible.
If I am correct in this conclusion, can I use two PQRs to increase the range qualified on the WPS?
How do I determine if I use the minimum thickness values of QW-403.6 or QW-451.1?