1
- #1
Kaadm
Mechanical
- Jun 28, 2012
- 32
Gents,
Attached are a photo of a self lubricated journal bearing installed on the drive end of a centrifugal pump driven by 5.5kv
motor.
The bearing failed after being heated up then the temeprature transmitter sent a high temperature alarm(setting alarm: 85 C).
I would be grateful if you could help me on finding the bearing failure causes based on the attached photos by interpreting
the impacts on it. Please note that only the lower half of the bearing which was affected.
Thank you.
Attached are a photo of a self lubricated journal bearing installed on the drive end of a centrifugal pump driven by 5.5kv
motor.
The bearing failed after being heated up then the temeprature transmitter sent a high temperature alarm(setting alarm: 85 C).
I would be grateful if you could help me on finding the bearing failure causes based on the attached photos by interpreting
the impacts on it. Please note that only the lower half of the bearing which was affected.
Thank you.