Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Bolt Hole Diameter Versus Anchor Bolt Diameter for Lug Supported Vessels 1

Status
Not open for further replies.

PressureVesselEngr

Mechanical
Joined
Mar 10, 2014
Messages
2
Location
US
Hello all,

I am reviewing a vertical vessel drawing with four support lugs. The drawing specifies to use 1" diameter bolts with a 11/8" anchor bolt diameter and I wanted some feedback if this is reasonable. Is there a standard table of bolt hole diameters for particular bolt sizes used in a lug supported vertical vessel in the ASME BPVC? Or is this more of a standard set from company to company? Any input would be greatly appreciated.

Thanks
 
Better to have a larger clearance hole, say 1 3/8, then supply a loose square washer 1 1/8 x 3/8 thick for field welding.
 
For standard anchor bolt chairs (chairs for uplift, not support of vessel), Megyesy's handbook shows holes 1/4" larger than the bolt size. Too small, and you run into tolerance issues, too large, and the nuts could be pulled through the holes.
 
Thank you tankman64 and JStephen for the feedback. I will take this into consideration and look into the details of Magyesy's Pressure Vessel Handbook.

Cheers,

PressureVesselEngr
 