nisha1980
Structural
- Feb 16, 2018
- 20
Hi
I have specified Hilti HSC-I safety anchors to fix structural door frame to the concrete wall. the grade of the bolts are specified as min 8.8/S bolts.these will be zinc plated countersunk bolts and still exposed. .
they advised they will use 12.9 grade bolts . My question is 12.9 the high tensile bolts is ok in terms of strength (UTS is 1200Mpa ). But the type of application usually use for mechanical assembly .
these property class 12.9 are susceptible to hydrogen pick up, possibly leading to delayed brittle fracture . hydrogen pick up can occur from pickling process used in galvanising or from rust formation in service. Specialist advise should be sought before specifying these bolts . and these are precision bolts and suitable for mechanical assembly. Use as fitted bolts ( from steel designers manual)
We do not use galvanising option , we can go with Zinc plated one.
Please let me know if you know about this and can we accept to use 12.9 grade bolts without considering the application?
Thanks in Advance
I have specified Hilti HSC-I safety anchors to fix structural door frame to the concrete wall. the grade of the bolts are specified as min 8.8/S bolts.these will be zinc plated countersunk bolts and still exposed. .
they advised they will use 12.9 grade bolts . My question is 12.9 the high tensile bolts is ok in terms of strength (UTS is 1200Mpa ). But the type of application usually use for mechanical assembly .
these property class 12.9 are susceptible to hydrogen pick up, possibly leading to delayed brittle fracture . hydrogen pick up can occur from pickling process used in galvanising or from rust formation in service. Specialist advise should be sought before specifying these bolts . and these are precision bolts and suitable for mechanical assembly. Use as fitted bolts ( from steel designers manual)
We do not use galvanising option , we can go with Zinc plated one.
Please let me know if you know about this and can we accept to use 12.9 grade bolts without considering the application?
Thanks in Advance