Beckipedia
Marine/Ocean
- Jun 20, 2011
- 3
Dear all
First time poster but Eng-tips has been a great resource to me recently.
Is there an adhesive or bonding for two polycarbonate sheets that will stay in seawater?
The sheets are about 12mm thick and need to stay put for up to 3-4 weeks.
I have been told that Cyanocrylate will work on dry land but it is water soluable so wouldn't under water.
Would Methylene chloride work?
Thank you in advance
Becky
First time poster but Eng-tips has been a great resource to me recently.
Is there an adhesive or bonding for two polycarbonate sheets that will stay in seawater?
The sheets are about 12mm thick and need to stay put for up to 3-4 weeks.
I have been told that Cyanocrylate will work on dry land but it is water soluable so wouldn't under water.
Would Methylene chloride work?
Thank you in advance
Becky