Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

bonding "Santoprene"

Status
Not open for further replies.

chopper75

Aerospace
Sep 27, 2011
95
We are trying to bond some rubber trim to the edge of steel sheet (.06"thk) with VHB tape. The tape holds well to the steel but doesn't want to bond to the rubber. The material is "Santoprene". Could someone recommend a good bonding tape we could use?
 
Replies continue below

Recommended for you

The rubber probably has a release agent on or in it. Prepare the surface properly for bonding. This would include abrasion with sandpaper or by sand blasting, solvent wipe, and plasma or flame treatment. Flame treatment can be as simple as lightly sweeping the surface with a propane torch. It is not the heat that is effective, but the highly reactive free-radicals in the flame.
 