Toufique
Aerospace
- Jan 27, 2024
- 1
Hello, I am looking for propagation data for the BS5S82 material (case hardened). I checked in MMPDS and ESDU but to no avail. does anyone know where I can find this data? Or at least similar materials in terms of propagation properties? It will be a great help. Thank you.