Hello users,
From Nominal stress-strain curve(compressive), I calculated logarithmic plastic strain using following formula.
Log plastic stain = Nominal strain - (true comp stress/E)
Is it right? I get ascending values till 75% strain then my log plastic strain descends. Abaqus asks for a value in ascending order. What is wrong with my calculation?
My calculation:
Nominal Stress Nominal Strain Nom.strn-(true strs/E)
0,24 0,05 0,013636364
0,27 0,1 0,059090909
0,3 0,15 0,104545455
0,32 0,2 0,151515152
0,34 0,25 0,198484848
0,35 0,3 0,246969697
0,38 0,35 0,292424242
0,4 0,4 0,339393939
0,43 0,45 0,384848485
0,47 0,5 0,428787879
0,51 0,55 0,472727273
0,58 0,6 0,512121212
0,67 0,65 0,548484848
0,82 0,7 0,575757576
1,07 0,75 0,587878788
1,54 0,8 0,566666667
True stress is equal to nominal stress since my poisson ration is zero.
Thanks for your time. Any help would be nice.
From Nominal stress-strain curve(compressive), I calculated logarithmic plastic strain using following formula.
Log plastic stain = Nominal strain - (true comp stress/E)
Is it right? I get ascending values till 75% strain then my log plastic strain descends. Abaqus asks for a value in ascending order. What is wrong with my calculation?
My calculation:
Nominal Stress Nominal Strain Nom.strn-(true strs/E)
0,24 0,05 0,013636364
0,27 0,1 0,059090909
0,3 0,15 0,104545455
0,32 0,2 0,151515152
0,34 0,25 0,198484848
0,35 0,3 0,246969697
0,38 0,35 0,292424242
0,4 0,4 0,339393939
0,43 0,45 0,384848485
0,47 0,5 0,428787879
0,51 0,55 0,472727273
0,58 0,6 0,512121212
0,67 0,65 0,548484848
0,82 0,7 0,575757576
1,07 0,75 0,587878788
1,54 0,8 0,566666667
True stress is equal to nominal stress since my poisson ration is zero.
Thanks for your time. Any help would be nice.