Having an intermittent issue with hardening 3.5 in OD, varies in length of 4150 steel. Can not find any variables with heat treatment/quenching/tempering process. In furnace at 1520F for 4 hours, oil quenched and then tempered at 1020 for 4 hours. Can get low hardness on pieces from batch that has acceptable pieces, all of which were done at the same time. Looking at carbon equivelancy, coming up with .88. Contemplating raising the temp to 1600F. Any thoughts?