Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Carbon steel tubes standard

Status
Not open for further replies.

Jay T

Mechanical
Mar 17, 2023
5
Hi I am looking for more understanding on some standards. For drawings of steel plates, we follow G40.21-44W. Does this apply to steel tubes too? or it is different?
 
Replies continue below

Recommended for you

What standard system are you using?
They all have an index where you can look up the titles and scopes of the specs.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
"Overview
"This seventh edition, two-part standard covers structural quality steel plates, shapes, hollow sections, sheet, sheet piling, cold-formed channels, Z sections, and bars for general construction and engineering purposes."

Check with local suppliers or fabricators to see what is commonly used and available, particularly in smaller quantities.
Note that structural tubing, mechanical tubing, and piping may all be different products.
 
HSS can be either G40.21 or A500. There are tolerance differences on the wall thickness. In my experience G40.21 is more expensive.
 