knightquestion
Civil/Environmental
- Jan 4, 2007
- 2
Have a petroleum waste water stream going into an existing treatment plant we are upgrading. All old below grade and exposed pipe is listed as ductile iron on old plans (late 60s, early to mid 70s). We will be replacing some pipe, and tieing into others. Some lines will be gravity, some are forced. Design life 30 years. Can someone give me a quick primer (or point me to one) on the use of each of these materials in ww jobs. What types of joints are best for below grade matches to the existing ductile. Thanks to the folks who can help!