I have heard of aftermarket performance cranks being described as "cast steel". I suspect they are nodular cast iron or austempered ductile iron. A cast steel crank would be unlikely, but not totally beyond the realm of possibility. Anyone know what these really are?
 
Replies continue below

Recommended for you

I have always presumed nodular cast iron, but I don't really know.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Nodular iron is preferred alloy,as it has lower density than steel, better machinability than steel,cost of production of nodular iron is lower compared to steel casting.

I shall be glad if steel castings are to be substituted,for that would mean good business for me.

Chocolates,men,coffee: are somethings liked better rich!!
(noticed in a coffee shop)
 
I did some googling and found several vendors that offer "cast steel crankshafts" made from "80-60-06" alloy. Not only is this nodular iron, rather than steel, but they didn't even get the designation right (it is 80-55-06). The "80" is normally dropped. Another case of marketing hype/ignorance. End of excercise.
 