I have a set of clegg impact values (CIV) which i have obtained and recorded and I need to convert them to %CBR Values.
I have used the following formula on each CIV that i have recorded and have the results from them.
% CBR = 0.07(IVxIV)
An example of a result I am getting are as follows:- 0.07(59 x 59) = 243.67
Does this mean that the CBR % is 243.67%? or am I wrong?
I have some Design Specifications that require CBR Value of 30% but all my results are throwing out HIGH readings after the equation so its throwing me alittle.
Can anyone help?
Thanks
I have used the following formula on each CIV that i have recorded and have the results from them.
% CBR = 0.07(IVxIV)
An example of a result I am getting are as follows:- 0.07(59 x 59) = 243.67
Does this mean that the CBR % is 243.67%? or am I wrong?
I have some Design Specifications that require CBR Value of 30% but all my results are throwing out HIGH readings after the equation so its throwing me alittle.
Can anyone help?
Thanks