Good morning all,

I wonder if you can share experiences about the neutralizer amine injection system used for your CDU overhead line?

Many facilities are still using conventional slotted angle quills for this application. As known, these can present several limitations, including:

- inconsistent mixing and flow of the chemical;
- Uncontrolled atomization and wide range of droplet sizes;
- increased risk of localized corrosion at the overhead line;
- improper or inefficient neutralization of the overheard CDU stream;

I wonder if someone has experience with the use of steam atomizing spray nozzles for this particular application. Any info on advantages, limitations and issues encountered would be appreciated.

Thanks in advanced for your support.
 
Replies continue below

Recommended for you

Thank you Luis.

I wonder if you are using such systems and what is your experience.

I truly appreciate your thoughts on this.

Regards,
Ricardo
 
When I was up to date on this subject, our CDU corrosion control was done by Baker Hughes automatic neutralizer dosing system, with conventional spray nozzles, whose proprietary neutralizer injection was done according to an on-line automatic pH analyzer. At that time we didn't have any major problems with this control.
 