snellen
Materials
- Jun 30, 2005
- 6
Before winter we supplied some CF8M "posts" for building entrance protection (9/11....). We cast them and sold them here in Boston. I just got a call saying that the side facing the road is rusting. I have yet to take a ride over there but I was wondering if you guys have any input? The parts have been heat treated and passivated. Keep in mind that last winter was about the worst in history for us.
Thanks in advance.
Gerard Snellen
Wollaston Alloys
Thanks in advance.
Gerard Snellen
Wollaston Alloys