PROCEDURE
4.3.1 Calibrate the meter, using the buffer solutions, in accordance with the manufacturer's
instruction manual.
4.3.2 Measure 11 ml of glycol sample and 239 ml distilled water into a 250ml beaker. Mix
thoroughly.
4.3.3 Place pH electrode and thermometer into the solution.
4.3.4 Adjust temperature compensation control on pH meter to correspond to solution
temperature.
4.3.5 Read pH directly from meter scale and record.
4.3.6 Rinse electrodes with distilled water
I do not figure out why to add distilled water for the test. the man made procedure already has retired.
I would appreciate your advice on the master.
thanks all in advance!
our gas processing has TEG generation system that required to check pH in lean TEG weekly.
the procedure to test pH of lean TEG as below:
PROCEDURE
4.3.1 Calibrate the meter, using the buffer solutions, in accordance with the manufacturer's
instruction manual.
4.3.2 Measure 11 ml of glycol sample and 239 ml distilled water into a 250ml beaker. Mix
thoroughly.
4.3.3 Place pH electrode and thermometer into the solution.
4.3.4 Adjust temperature compensation control on pH meter to correspond to solution
temperature.
4.3.5 Read pH directly from meter scale and record.
4.3.6 Rinse electrodes with distilled water
I do not figure out why to add distilled water for the test. the man made procedure already has retired.