Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Chrome Plating after Ultrasonically Welding

Status
Not open for further replies.

breezy83

Mechanical
Sep 22, 2020
16
Has anyone had success with chrome plating on 2 plastic (ABS plating grade) parts that have been ultrasonically welded together? I received DFM feedback from 1 vendor that said they thought there would be discoloration around the seam due to an inability to properly clean that area. I would appreciate any feedback! Thanks!
 
Replies continue below

Recommended for you

Your vendor is likely to be correct.



Politicians like to panic, they need activity. It is their substitute for achievement.
 