Sep 2, 2011 #1 Erik2249 Mechanical Aug 25, 2009 4 0 0 CH I am looking for information about the coeffient of (thermal) expansion of this nickle based alloy that is used for rotors of Waukesha pumps. I want to compare this to Stainless steel 316 / 316L.
I am looking for information about the coeffient of (thermal) expansion of this nickle based alloy that is used for rotors of Waukesha pumps. I want to compare this to Stainless steel 316 / 316L.
Sep 2, 2011 1 #2 A Artisi Mechanical Jun 11, 2003 6,458 0 36 AU Have you considered asking Waukesha? It is a capital mistake to theorise before one has data. Insensibly one begins to twist facts to suit theories, instead of theories to suit facts. (Sherlock Holmes - A Scandal in Bohemia.) Upvote 0 Downvote
Have you considered asking Waukesha? It is a capital mistake to theorise before one has data. Insensibly one begins to twist facts to suit theories, instead of theories to suit facts. (Sherlock Holmes - A Scandal in Bohemia.)
Sep 2, 2011 1 #3 ione Mechanical Oct 22, 2009 1,342 0 0 IT 8*10^(-6)inch/(inch*F) in the range grom 32 to 212 F Upvote 0 Downvote