Cold & Hot Allowable Stress for A778 304L pipe 3

Status
Not open for further replies.

ellas1

Structural
Dec 20, 2011
28
What is the Cold & Hot Allowable Stress for A778 304L pipe. I cannot find this material on B31 tables.

Thank you
 
Replies continue below

Recommended for you

Which B31 code section do you require?

Huub
- You never get what you expect, you only get what you inspect.
 
I am not looking for B31 code. I am looking for the allowable stress for this material because it is not listed on B31. Th elates t I have is 2018.

Thank you
 
Ellas1,
What is the hot/design temperature?

GDD
Canada
 
B31.1, B31.3, B31.?? It will determine whether and how you might an unlisted material.

Huub
- You never get what you expect, you only get what you inspect.
 
I don't believe that you can use A778 because it is unannealed product.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 