Dear all,
There is two rebar in a row with lapping length, 100mm.
In case that I cannot follow the standard length of anchorage length and lapping length of rebars, can I consider the as the following?
(lapping length is considered as anchorage length)
Tension force = 300kN
Rebar
a) Dia : D20
b) fbd = 3Mpa
c) Anchorage length : 300mm
d) lapping length : 100mm
e) Total anchorage length = 400mm
=> F, (Rebar resist agaist tension) = fbd x L(300+100) x Perimetre of rebar = 377kN
There is two rebar in a row with lapping length, 100mm.

In case that I cannot follow the standard length of anchorage length and lapping length of rebars, can I consider the as the following?
(lapping length is considered as anchorage length)
Tension force = 300kN
Rebar
a) Dia : D20
b) fbd = 3Mpa
c) Anchorage length : 300mm
d) lapping length : 100mm
e) Total anchorage length = 400mm
=> F, (Rebar resist agaist tension) = fbd x L(300+100) x Perimetre of rebar = 377kN