We have a 15 KV system with insulated bus (powder bed epoxy-60 mils) and G10 glass epoxy supports with silicone rubber inserts. The phase to phase spacing is 5-3/8” and the phase to ground is 3-1/2”. This was installed around Sept./Oct,2001!! We now see white powder forming around the support areas along the full lenght of the bus run and in some locations with the existing GPO3 glastic supports, we have visible tracking!
The application is indoor, clean, dry (filtered and ac). THe load is appox 500amps on the bus.