Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cozzone Curves- Where can they be found? 6

Status
Not open for further replies.

realJedi

Mechanical
May 17, 2004
4
Hello all,

I'm looking for Cozzone curves for use with the Fb=Fm+Fo(K-1) equation, but need more curves than is shown in Bruhn. Does anyone know where they can be found? And better yet are they online to be downloaded/copied?

Thanks for the help.....
 
Replies continue below

Recommended for you

What are you looking for specifically? Do you need more 'K' values or more values of fo?

Are you trying to solve a particular problem, or are you just compiling reference data?

SuperStress
 
Superstress,

I'm looking to compile reference data for values of Fo for solving problems with precipitation hardening stainless steels, ferritic and austenitic stainless steels. However what I'm really after are the values of Fb and need Fo to calculate.

My current need is to find a reference for 17-4PH at H900.


A little off topic but, similarly, I understand that Ramberg-Osgood curves yeild similar values for Fb without the need for values of Fo?
 
Here are the equations for fo. I put these into a spreadsheet for quick calculations. This is a little complicated, but I think this will be comprehensible...

fo/Ftu=6/eu2*{1/3*(Ftu/E)2+eu'*((m+1)/(m+2))*(Ftu/E)+(m/2m+1)*(eu')2}-2

where:

m=log(eu'/.002)/log(Ftu/Fty)

and

eu'=eu-(Ftu/E)

Where:

eu=elongation
E=Young's modulus
Ftu,Fty are ultimate and yield values in tension.

In case that's not confusing enough, here are my spreadsheet entries; you should be able to cut-and-paste these into Excel and get an answer.

For this spreadsheet, the following variables are defined in these locations:

B2=E, Young's modulus
B3=Ftu, ultimate tensile strength
B4=eu, elongation (e.g. 7%=.07)
B5=eu'=B4-B3/B2
B6=Fty, yield strength in tension
B7=m=LOG(B5/0.002)/LOG(B3/B6)
B8=fo/Ftu=(6/(B4^2))*((B3/B2)^2/3+B5*(B7+1)/(B7+2)*B3/B2+(B7/(2*B7+1))*B5^2)-2
B9=fo=B8*B3


That should work, if I've managed to transcribe it correctly. By the way, the reference for this is McDonnell Aircraft Report 339, 2 January 1969, Revised 1 December 1971, page 14.02.

Let me know if it doesn't work and I'll check my equations again to make sure I didn't fat-finger it.

SuperStress
 
Hi all

Regarding references for additional material curves for the Cozzone method, Lockheed employs this method in SMM 53d (SMM is the Structures Methods Manual) and published additional data for all their methods for each of the Mil Handbook versions in supplemental Lockheed Reports (ie LRXXXXX). The one I believe I have used in the past was called LR31445 entitled "Stress Memo Curves for Materials in Mil-Hdbk-5E". If you can borrow one from someone you will find addtional curves for plastic bending for: 2024,2090,2124,6061,7050,7075,7175,7475,7049,Ti6al4v,inconel,15-5ph,17-4ph,13-8ph,300m,A356,A357,etc. and for various product forms.

Good hunting

JB
 
Hi,

In Table C3.2 at page C3.11 of Bruhn's book, there is a fo value for Yield strengh.

I am wondering if there is a corresponding formula such as "fo/Ftu=6/eu2*{1/3*(Ftu/E)2+eu'*((m+1)/(m+2))*(Ftu/E)+(m/2m+1)*(eu')2}-2" for the yield strength?

Thank you.

laotseng
 