Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Creep Analysis in Abaqus

Status
Not open for further replies.

Rohan Ahrawal

Student
Dec 8, 2024
2
I'm performing a creep analysis on a dogbone specimen made of SS-304. I am following this paper Correlation Analysis of Established Creep Failure Models through Computational Modelling for SS-304 Material.

Following is the geometry:
Screenshot 2024-12-08 162258.png
In property module I've created the material, specifying Young's modulus (201000 MPa) and Poisson's ratio (0.31) on sheet "Elastic" and specifying Power Law Multiplier (6.18e-17), equation stress order (6.82) and time order (0) in sheet "Creep".

Then I create Visco step in Step module, specifying a time period of 6480000 sec (18000 Hr); in the sheet "Incrementation" I've chosen the max number of increment (10000), Initial increment size (1), minimum (1e-20) and max (360000), then I've chosen creep/swlling...tolerance (0.1).

After that I've created a coupling constraint in Interaction module, then a reference point for the whole grip section with neck section of the specimen.

Screenshot 2024-12-08 165128.png

I've created a symmetry BC for the bottom section of grip and neck.

Screenshot 2024-12-08 165251.png

Then I've defined a load (displacement) of 2mm Magnitude. Also a thermal field is also defined of 720°C.

Screenshot 2024-12-08 165410.png

I've done the mesh, I’ve created and started the job, but I am getting wrong stress results but the creep results are somewhat In line. More over the creep curve trend also matched that of the literature, But not for stress results,

Screenshot 2024-12-08 165928.pngScreenshot 2024-12-08 170448.pngScreenshot 2024-12-08 165943.pngScreenshot 2024-12-08 170519.png

Any suggestion on how to fix the problem.
 
Last edited:
Replies continue below

Recommended for you

One image is missing. It's much better to upload images directly here instead of using 3rd party hosting services where files may disappear after some time.

So you took one material model case from the article. BCs seem to be applied differently in your model. Exactly which figures from the article are you using for comparison ? Is Figure 6 one of them ?
 
One image is missing. It's much better to upload images directly here instead of using 3rd party hosting services where files may disappear after some time.

So you took one material model case from the article. BCs seem to be applied differently in your model. Exactly which figures from the article are you using for comparison ? Is Figure 6 one of them ?
While modelling I also thought that I might be using wrong BCs. In the paper it is written "One end of the specimen was fixed, and the displacement was set at the other end with an amplitude of 2 mm/min". I am not quite understanding it. And for material properties I have only specified elastic and creep properties for SS-304 do I need to specify density, thermal expansion and other properties?
 
In the paper it is written "One end of the specimen was fixed, and the displacement was set at the other end with an amplitude of 2 mm/min". I am not quite understanding it.
Yes, this paper is quite unclear, especially when it comes to the description of the setup. That’s unfortunately quite common in scientific articles.

They mention velocity here but then write about steady (force?) load which makes sense for creep analysis.

It might be difficult to properly recreate the results from this paper with such unclear and limited descriptions.

And for material properties I have only specified elastic and creep properties for SS-304 do I need to specify density, thermal expansion and other properties?
You need density only for inertia effects and thermal expansion only if you want to take this effect occuring due to temperature change into account.
 