I have to cut a 2-4" Acme screw thread on a shaft and make 2 mating nuts to match. I made a "go" gauge so that as soon as the "go" gauge is able to fit into the nut I know that I have the proper clearances. The "go" gauge was made slightly larger than a standard shaft would be. The problem occurred when the "go" gauge went into the nut the major diameter of the nut was .040 bigger than it should be.
Sizes:
Major Dia of go gauge: 2.020 (Min of Major dia of nut)
Minor Dia of go gauge: 1.750 (Min of Minor dia of nut)
Major Dia of Nut: 2.078 (Min 2.020 Max 2.040)
Minor Dia of Nut: 1.754/1.756
Any help would be appreciated. Thank you..
Sizes:
Major Dia of go gauge: 2.020 (Min of Major dia of nut)
Minor Dia of go gauge: 1.750 (Min of Minor dia of nut)
Major Dia of Nut: 2.078 (Min 2.020 Max 2.040)
Minor Dia of Nut: 1.754/1.756