affa289
Industrial
- Jul 10, 2017
- 9
Hey guys only new really to laser cutting every thing has been going ok but today when cutting some 8mm plate I had this happening I don't know is it cut speed focus power hahahah has me a bit stumped
Thanks for any help
Matt
Thanks for any help
Matt