braham0793
Mechanical
- Sep 3, 2015
- 36
Dear ;
Good afternoon,
A client has asked me to reinforce 4 ships, I am doing the relevant reviews and I have found the following surprise:
The beam that works as a column has been deformed. According to what my client indicates is because they had problems when mounting the roof and therefore had to deform the column (beam) so that both the base and the roof have the Same measure.
My question is the following:
The column will not be negatively affected if it is straightened by the use of heat ?.
Consider that the column is 5 years old.
Best regards.
Good afternoon,
A client has asked me to reinforce 4 ships, I am doing the relevant reviews and I have found the following surprise:

The beam that works as a column has been deformed. According to what my client indicates is because they had problems when mounting the roof and therefore had to deform the column (beam) so that both the base and the roof have the Same measure.
My question is the following:
The column will not be negatively affected if it is straightened by the use of heat ?.
Consider that the column is 5 years old.
Best regards.