We have a WPS for Stainless Steel that was supported by PQR with backing gas. We used this WPS to weld plate with thickness ranging from 1.5mm - 2.4mm.
If we are going to deleted/remove backing gas and no root gap (square joint), do we need to make a new PQR?
As per ASME IX ed. 2013:
QW-200.1
(c) Changes to the WPS. Changes may be made in the nonessential variables of a WPS to suit production requirements without requalification provided such changes are documented with respect to the essential, nonessential, and, when required, supplementary essential variables for each process. This may be by amendment to the WPS or by use of a new WPS.
Table QW-256: 408.5 refers to the deletion or change in backing flow is nonessential varialble.
QW-408.5 The addition or deletion of gas backing, a change in backing gas composition, or a change in the specified flow rate of backing gas.
QUESTIONS: with regard to the DELETION/REMOVAL of backing gas for the actual work condition:
1. Is it correct to say that referring to Table QW-256 we can change our WPS without the re-qualification of the PQR?
2. Does QW-408.8 refers to the deletion of backing gas?
Please correct me if I am wrong.
Thank you
If we are going to deleted/remove backing gas and no root gap (square joint), do we need to make a new PQR?
As per ASME IX ed. 2013:
QW-200.1
(c) Changes to the WPS. Changes may be made in the nonessential variables of a WPS to suit production requirements without requalification provided such changes are documented with respect to the essential, nonessential, and, when required, supplementary essential variables for each process. This may be by amendment to the WPS or by use of a new WPS.
Table QW-256: 408.5 refers to the deletion or change in backing flow is nonessential varialble.
QW-408.5 The addition or deletion of gas backing, a change in backing gas composition, or a change in the specified flow rate of backing gas.
QUESTIONS: with regard to the DELETION/REMOVAL of backing gas for the actual work condition:
1. Is it correct to say that referring to Table QW-256 we can change our WPS without the re-qualification of the PQR?
2. Does QW-408.8 refers to the deletion of backing gas?
Please correct me if I am wrong.