Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Differences between Pipe, API 5L X42 Psl1 and Pipe, Api 5L X42 Psl2 1

Status
Not open for further replies.

brvs2014

Mechanical
May 15, 2017
33
Differences between Pipe, API 5L X42 Psl1 and Pipe, Api 5L X42 Psl2
 
Replies continue below

Recommended for you

Look at API 5L. Too many to list, but basically PSL2 is tighter on various things like composition and some material properties.

Most pipelines are made from PSL2 IMO.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
He's right as usual. Nobody uses 1 anymore. Use PSL2

"He's declaring war on the planet itself."- Vicente Fox
 
It is from the API 5L 2004 edition, but i've used it as a reference a few times back in the fab shop days.


Capture_j7bjrd.png
 
Great.
Yes PSL2 requires tracibility, fracture toughness and prohibits repairs. Those are most important differences for me.

Richard Feynman's Problem Solving Algorithm
1. Write down the problem.
2. Think very hard.
3. Write down the answer.
 
PSL1 does not comply with the PED whilst PSL2 does
 