Hi guys!
I found discordance between B31.1 Table 132.1.1-1 and ASME BPVC Sec.8 UCS-56, So I ask you which one should apply.
In Table 132.1.1-1 of B31.1 2018 Ed., control thickness is criterion for PWHT.
But in UCS-56 of ASME BPVC Sec.8 2021 Ed., nominal thickness is criterion for PWHT.
And for P-15E, "Weld Thickness(Nominal)" is criterion for PWHT.
I'm so confused because those two thickness are different.
Could you tell me which one is correct?