I have a question about the impact testing per ASME Section VIII Div 2 section 3.11.4. of SA-240 304L material for a vessel with a design MDMT of 20F.

The way I understand it is that the material is impact tested or the production impacts of Category A and B joint are tested. I do not see any exemption for no impact test. Is this correct or am I missing something.
 
Replies continue below

Recommended for you

Curly,
Have you reviewed the exemptions in par 3.11.4.3?
 
If you check 3.11.4.3, 3.11.4.4, and 3.11.4.5, they all exempt 304L material from impact testing above -20°F. It is very uncommon to require impact testing of austenitic stainless steels except for very low temperatures.
 
Ok I missed that 3.11.4.2 was for thermally treated plates.

Also I looked and the vessel is rated at MDMT is -55F but this is still in the exempt range.

Thanks for the replys.
 