Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations pierreick on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

DUESENBERG RADIATOR SHELL AND GRILL

Status
Not open for further replies.

duesey

Automotive
May 15, 2006
1
Does anyone have any ideas or tips on how I may duplicate the classic Duesenberg radiator shell and grill? I want to build a replicar , and start with the rad grill and shell. How do I form it? THANKS.
 
Replies continue below

Recommended for you

If you're planning on building a replica then you need to do some serious groundwork. I build grills,radiators,windscreens & chassis's for various replica's and as reproductions for original vehicles.Until you have done some planning building a grill shell is not going to get you very far.If you want to make the grill shell start with some good dimensions and drawings/photo's and make a wooden buck, then pattern off the buck for your metal parts, tack it,weld it, & dress it up. I presume it will be steel and chrome plated. Hope this helps.
 
it is possible to take a nickle shell (like that from a 30-31 model A) and silver solder mods. Then have it coppered and plated. I did it once for a guy who was building a T-bucket. Turned out Ok. The advantage is you can use other platables and solder it to the shell too.
 