Hi guys - First post on this forum. I am in Aghanistan doing some project management and engineering for a clinic that is being built in a very small village in Helmand Province. The design calls for an above ground water tank made of 3/4 inch cast iron that will be charged by a local water well. Ground water here tends to be on the briny side with a salt content high enough that the locals can taste it and will generally avoid it if they can. Anyway, what I need to know is whether the brine will have a corrosive effect on the cast iron and any alternatives that you think appropriate. Thanks in advance guys.