albanbulku
Mechanical
- Mar 5, 2013
- 30
Please if someone can inform me about Hydro test frequency and if it is mandatory for each pipe according to this standart???
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
EN 10217-1 said:8.4.3.1 Leak-tightness
The tubes shall pass a hydrostatic test (see 11.8.1) or electromagnetic test (see 11.8.2) for leak-tightness.
Unless Option 6is specified the choice of the test method is at the discretion of the manufacturer.
Option 6: The test method for verification of leak-tightness in accordance with 11.8.1or 11.8.2is specified
by the purchaser.
NOTE SAW tubes cannot be tested in accordance with 11.8.2