Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

EN8D axle shafts temper time

Status
Not open for further replies.

thejackal3

Automotive
Mar 4, 2012
36
We do induction heat treatment of axle shafts made of EN8D and then furnace temper it.Axle shafts are 58-62 HRC as quenched.for how much time and at what temperature we temper them to get 55-56HRC on surface?
 
Replies continue below

Recommended for you

Assuming a belt furnace, 45-60 minutes for one hour at 350-375F would be the norm for induction hardened axle shafts.
 
thejackal3,it will,help,if you provide your thermal cycle details in the initial post,rather than providing them after someone responds. This will avoid wastage of time and discussions . Also,it will generate more meaningful response.

_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
 