I am woking on a job where I specified Simpson SET epoxy for some shallow, 1/2" anchors (2 1/4" embedment due to embedded slab items). I used the Simpson tables which gave me an allowable pullout of of 1805 lbs (ASD) at 2 1/8" embedment in 2000 psi concrete. The contractor used Hilti RE100 instead. Their tables do not go below 2 3/4" embedment with no reductions allowed. The owner is asking for an appendix D calc. The epoxys are similar with the Simpson bond being 10% stronger (3300 psi versus 3000 psi). My demand is only 1400 lbs (ASD). I assume concrete breakout is the actual failure mode so the bond strength should not be an issue. Is it reasonable to assume that the Hilti product will perform similarly.