Dear all,
I am looking for information about paint system applied under thermal insulation for subsea structures (FLET, ILT...)
With previous investigations 2 paint systems seems to match regarding the technical constraints
- 2 coats Sigmatherm 230 DFT 150µm for each coat
- 2 coats Thermaline 400 DFT 150µm for each coat
But I can’t find any track records for these paint system in previous project and I need to justify they are field proven paint systems.
Did you use these paints systems in previous project or did you meet these products for subsea structures?
I am not stick with PPG or Carboline, main constraints are :
- 2 coats 150 microns each
- phenolic epoxy
- Under thermal insulation with Temp up to 120°C
- Subsea structures
If you have any paint systems field proven which match these points....
Regards
Marc
I am looking for information about paint system applied under thermal insulation for subsea structures (FLET, ILT...)
With previous investigations 2 paint systems seems to match regarding the technical constraints
- 2 coats Sigmatherm 230 DFT 150µm for each coat
- 2 coats Thermaline 400 DFT 150µm for each coat
But I can’t find any track records for these paint system in previous project and I need to justify they are field proven paint systems.
Did you use these paints systems in previous project or did you meet these products for subsea structures?
I am not stick with PPG or Carboline, main constraints are :
- 2 coats 150 microns each
- phenolic epoxy
- Under thermal insulation with Temp up to 120°C
- Subsea structures
If you have any paint systems field proven which match these points....
Regards
Marc