Magnet Length Width Thickness Surface Field Pull FORCE
(Gauss) (LB)
B444 1/4 " 1/4 " 1/4 " 5754 4.25
B666 3/8 " 3/8 " 3/8 " 5754 10.07
B888 1/2 " 1/2 " 1/2 " 5754 18.71
BCCC 3/4 " 3/4 " 3/4 " 5754 40.59
BX0X0X0 1 " 1 " 1 " 5754 76.41
What explains this?
Is the attraction force determined from the surface field?
A larger magnet would have the equal value fore the surface field but a stronger attraction/repulsion force?!