Dear experts
In my project , equipment nozzle of 22mm thickness with stud connection ( field weld) delivered to site with U stamp .Contractor carried out welding with piping as per project ITP and want to claim the first circumfertial joint belongs to piping code .
1. As per U-1 (e)(1) (a) the joint belongs to equipment code ASME DIV VIII . If it belongs to equipment code field welding activities , data reports , AI involvement all will be required. Is it right ?
2. In MDR , attachment details specified about nozzle details and in flange mentioned as N.A ,and no where mentioned about field welding. Shall this statement can be taken as joint belongs to piping code ?
For your valuable advises .
Thanks
Abraham
In my project , equipment nozzle of 22mm thickness with stud connection ( field weld) delivered to site with U stamp .Contractor carried out welding with piping as per project ITP and want to claim the first circumfertial joint belongs to piping code .
1. As per U-1 (e)(1) (a) the joint belongs to equipment code ASME DIV VIII . If it belongs to equipment code field welding activities , data reports , AI involvement all will be required. Is it right ?
2. In MDR , attachment details specified about nozzle details and in flange mentioned as N.A ,and no where mentioned about field welding. Shall this statement can be taken as joint belongs to piping code ?
For your valuable advises .
Thanks
Abraham