radaes
Mechanical
- Feb 14, 2005
- 36
We're trying to get some valves manufactured in Germany, but our drawings have a material spec for SA 53 and SA 105 and that doesn't mean anything to our German machinist. Anyone have the equivalent material numbers for Germany?
As far as I've been able to tell, SA 53-A seamless is Material Number 1.0308 - does that ring a bell for anybody? I've come up dry on the SA 105. Since it's entirely possible that the exact equivalent to SA 53/105 is an "exotic" in Germany, anyone know a common euro alternate or substitute?
Thanks for the help
cheers,
rad
"According to my calculations the problem doesn't exist."
As far as I've been able to tell, SA 53-A seamless is Material Number 1.0308 - does that ring a bell for anybody? I've come up dry on the SA 105. Since it's entirely possible that the exact equivalent to SA 53/105 is an "exotic" in Germany, anyone know a common euro alternate or substitute?
Thanks for the help
cheers,
rad
"According to my calculations the problem doesn't exist."