Ehiman1

Civil/Environmental
Oct 17, 2014
59
Good evening,
If I have to do a fatigue calculation about pressure vessel due to high temperature, How Can I do?
I can't use ASME VIII div.2 because I have temperature higher than ASME table values, but fortunately we aren't out of creep for the material.

Many thanks to Everyone for helping me
 
Replies continue below

Recommended for you

What is your material? What is your temperature?
 
try EN 12952-3 annex B and annex C

"...when logic, and proportion, have fallen, sloppy dead..." Grace Slick
 
Thank you for your answers!
It's stainless steel 316 at 495 °C.

I would like studying better this topic, but I can't find out a book about this.
Could you suggest me a pdf book or something else?
 
Check out ASME Section III, Division 5.
 