I have a project with a customer requirement of FN between 3 & 10 for the combination of 347SS and 310SS using ER309L filler. At 1st glance, I thought that would be easy to meet since it's a common range for Austinitic SS, but looking further into it, I see threads in this forum stating that 309 & 310 both are often very stable and have zero ferrite formation. If that's the case, then the 347/310 combination could have a lower FN that I'd originally thought.
I found an online tool for the Schaeffler diagram. The resulting FN varied greatly depending on dilution. I could ask what a typical expected dilution for multipass TIG welds would be, but I'm sure the answers would start with "It depends".
What recommendations do you have for the joining of these materials so that we meet the FN requirements?
I found an online tool for the Schaeffler diagram. The resulting FN varied greatly depending on dilution. I could ask what a typical expected dilution for multipass TIG welds would be, but I'm sure the answers would start with "It depends".
What recommendations do you have for the joining of these materials so that we meet the FN requirements?